Decay resistance, physical, mechanical, and thermal properties of heated oriental beech wood

dc.contributor.authorAydın, Emrah
dc.contributor.authorBaysal, Ergun
dc.contributor.authorToker, Hilmi
dc.contributor.authorTürkoğlu, Türker
dc.contributor.authorDeveci, İlyas
dc.contributor.authorÖzçifçi, Ayhan
dc.contributor.authorPeker, Hüseyin
dc.date.accessioned13.07.201910:50:10
dc.date.accessioned2019-07-16T08:22:21Z
dc.date.available13.07.201910:50:10
dc.date.available2019-07-16T08:22:21Z
dc.date.issued2015
dc.departmentAydin, E., Mugla Sitki Kocman University, Faculty of Technology, Department of Wood Science and Technology, Mugla, 48000, Turkey -- Baysal, E., Mugla Sitki Kocman University, Faculty of Technology, Department of Wood Science and Technology, Mugla, 48000, Turkey -- Toker, H., Mugla Sitki Kocman University, Faculty of Technology, Department of Wood Science and Technology, Mugla, 48000, Turkey -- Turkoglu, T., Mugla Sitki Kocman University, Koycegiz Vocational School, Department of Forestry, Mugla, 48800, Turkey -- Deveci, I., Mugla Sitki Kocman University, Faculty of Science, Department of Chemistry, Mugla, 48800, Turkey -- Ozcifci, A., Aksaray University, Faculty of Engineering, Department of Industrial Engineering, Aksaray, 68100, Turkey -- Peker, H., Artvin Coruh University, Faculty of Forestry, Artvin, 08000, Turkey
dc.description.abstractHeat treatment of Oriental beech (Fagus orientalis) wood was carried out by hot air in an oven for 2, 6, and 10 h at 125, 155, and 185°C. After heat treatment; decay resistance, oven dry density, modulus of rupture (MOR), compression strength parallel to grain (CSPG), and thermal characteristics of Oriental beech wood were investigated. Our results showed that heat treatment caused a decrease in oven dry density values of Oriental beech wood specimens. Heat treatment improved decay resistance of Oriental beech wood. Moreover, higher temperature and durations resulted in lower mass loss of wood after decay test. MOR values of heated Oriental beech decreased with increasing temperature and durations. CSPG values of Oriental beech decreased after heat treatments except for 2 and 6 hours heating at 125°C. According to the thermal analysis results, thermal properties of heated Oriental beech wood were preserved except for heated Oriental beech wood at 185°C for 6 and 10 hours.
dc.identifier.endpage928en_US
dc.identifier.issn1336-4561
dc.identifier.issue6en_US
dc.identifier.scopusqualityQ2
dc.identifier.startpage913en_US
dc.identifier.urihttps://hdl.handle.net/20.500.12451/2538
dc.identifier.volume60en_US
dc.identifier.wosqualityN/A
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.language.isoen
dc.publisherStatny Drevarsky Vyskumny Ustav
dc.relation.ispartofWood Research
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.subjectCSPG
dc.subjectDecay resistance
dc.subjectHeat Treatment
dc.subjectMOR
dc.subjectOriental Beech
dc.subjectOven Dry Density
dc.subjectThermal Characteristics
dc.titleDecay resistance, physical, mechanical, and thermal properties of heated oriental beech wood
dc.typeArticle

Dosyalar

Orijinal paket
Listeleniyor 1 - 1 / 1
Yükleniyor...
Küçük Resim
İsim:
aydin-emrah-2015.pdf
Boyut:
602.55 KB
Biçim:
Adobe Portable Document Format
Açıklama:
Tam Metin / Full Text